Alloy Steel Sheet and Plate

  • Home
  • Alloy Steel Sheet and Plate

Alloy Steel Sheet And Plate Manufacturer in India

alloy-steel-sheet
alloy-steel-plate

Specification Of Alloy Steel Sheet and Plate

ASTM Specification ASTM A240 / ASME SA240
Standard MSRR, AMS, BS, ASTM A240 / ASME SA240
Length & Sizes 1000 mm x 2000 mm, 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1250mm x 2500mm, 1500mm x 3000mm to 6000mm, 2000mm x 4000mm to 6000mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm, 2m, 2.44m, 3m, 36" X 120" or 48" X 144", 4' x 8', Cut to size available
Thickness 0.1mm to 100 mm Thk
Width 10-2500mm
Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.
Temper Annealed
Condition Polished on both sides
Finish Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Stock in form of Plate, Sheet, Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Clad Plate, Rolling Sheet, Flat Sheet, Rolling Plate, Flat Shim, Blank (Circle), hot rolled, cold rolled, annealed, soft annealed, descaled, sheared, tread plate, Checker Plate
Value Added Service Cladding, Heat Treatment, Annealed, Pickling, Polish, Rolling, Cutting, Bending, Forging, Minor Fabrication Etc.
Test Report
  • Raw Materials Certificate
  • EN 10204/3.1B
  • 100% Radiography Test Report
  • High special strength, high melt point
  • Third Party Inspection Report, etc
  • Excellent corrosive resistance, good thermal resistance
  • Customer support after-sales service
  • Strict Control from Raw Material to Finished

Dimension of UNS N08020 Plate

Metric Dimensions

Surface finish Thickness (mm) Width (mm)
2B – Cold rolled, heat treated, pickled, skin passed 0.25–8.0 max. 2032
2D – Cold rolled, heat treated, pickled 0.4–6.35 max. 1524
2E – Cold rolled, heat treated, mechanically descaled 0.4–8.0 max. 2032
2R – Cold rolled, bright annealed 0.25–3.5 max. 1524
2H – Work hardened 0.4–6.35 max. 1524
Polished, brushed 0.5–4.0 max. 1524

Imperial Dimensions

Surface finish Gauge (in) Width (in)
2B – Cold rolled, heat treated, pickled, skin passed 10–24 max. 72*
2D – Cold rolled, heat treated, pickled 12–24 max. 60
BA Mexinox only 18–28 max. 48
Polished (not brushed) 11–24 max. 60
Temper rolled Mexinox only 13–29 max. 48

Chemical Properties of Alloy Steel Sheet and Plate

Alloy 20 Ni C Mo Mn Si Fe Cu S P Cr
32 – 38 0.02 max 2 – 3 1 – 2 0.7 max Bal 3 – 4 0.005 max 0.02 max 19 – 21

Mechanical Properties of Alloy Steel Sheet and Plate

Density Melting Point Yield Strength (0.2%Offset) Tensile Strength Elongation
8.1 g/cm3 1443 °C (2430 °F) Psi – 35000 , MPa – 241 Psi – 80000 , MPa – 551 30 %